1. … low hydrogen content when combined with Ceweld  FL 155. Developed for welding cold tough, high tensile fine grain steel exceeding a yield …
  2. … temperature should be between 100°C (212 °F) and 150°C (302 °F) . As welding flux FL 155 should be used because of its high basicity and low …
  3. … A high basic electrode for welding austenitic-ferritic stainless alloys of the 22% Cr, 5% Ni, 3% …
  4. … tungsten tool tips. Very good weld deposit appearance and outstanding welding properties on both AC and DC+. Preheating is not required. … …
  5. … draad met waterstof lager dan 3 ml/100gr lasmetaal was de basis voor deze nieuwe ontwikkeling. Onder de noemer Megafil 890R is deze …
  6. … CEWELD® SG CrMnMo EN 4332: FE-WL1805 (8CrMnMo12-4-9) wire is used for welding matching, and similar, composition base materials. … 30CrMoV12, …
  7. … treatable. Thicker sections should be preheated (150°C) prior to welding. … AlMgSi 0, AlSiMg (A), AlSi 1 MgMn, AlMg1SiCu, 3.3206, …
  8. … excellently suitable for root runs in vertical up position in pipe welding. The slag is self detaching and the special red coating was …
  9. … Ductile welding deposit with good sliding properties suitable for bearings etc. …
  10. … Mo content, with low carbon content (less than 0.05%), to be used for welding creep resistant steels. … For 2.5%Cr-1%Mo-alloyed, …