1. … good ductility after prolonged exposure at temperatures of 1200, 1400, 1600F (650, 760 and 870°C) for 16,000 hours. … Alloy HX, X, Nickel …
  2. … CEWELD® 320 Tig was designed specifically to withstand sulfuric acid. Its nickel, chromium, molybdenum and copper levels all …
  3. … alkalis, and some molten salts. It is especially suitable in many sulfuric, nitric, hydrochloric, and acetic acid applications. Backup …
  4. … In case of sensitive base material preheating is recommended at 300-400°C. Old Hardfacing layers should be removed, clean or grind properly …
  5. … and suitable for applications when exposed to hydrogen sulfide or sulfur dioxide. … The nominal composition (wt.-%) of filler metal of this …
  6. … corrosion due to the high CrMo(N) content (Pitting index > 40). Furthermore, the weld metal alloy is saltwater-proof and offers high …
  7. … and a Ni-based alloy. Crushed cast carbide will guaranty a long life. Furthermore the Ni-based alloy provides an excellent corrosion …
  8. … corrosion resistance against delude hot acids. Suitable for use up to 400°C. SA 317L is best to be used in combination with FL 838 … 1.4429, …
  9. … are used for fabrication of equipment and vessels for handling of sulfuric acid and many chloride containing media. This fluxcored wire may …
  10. … than AISI 316 due to the high Mo. content. Suitable for use up to 400°C … 1.4429, 1.4434, 1.4435, 1.4436, 1.4438, 1.4439, 1.4453, …