1. … welding pool without spatter loss, easy slag release, very nice bead surface … Reh ≤ 420 MPa ISO 15608: 1.1, 1.2 1.0426, 1.0429, 1.0481, …
  2. … creep strength are kept above the minimum considered necessary to ensure satisfactory performance. In this case, weldments will be weakest …
  3. … a tough, ductile, wear-, corrosion-, and high-temperature resistant surface. The hardness of 30% cold-worked wrought product is … overlay •"Make/break" seal welds in threades unions •Weld overlays to marine riser tensioners, shafts, and larger hydraulic systems pistons …
  4. … that of 304 stainless steel, DUR12 can be used to protect bearing surfaces in non-lubricating conditions due to its resistance to … plastic, wood and paper as well as high stressed sealings and, sliding surfaces. … DUR 12 Tig … A 5.21: ERCoCr-B … 14700: S Co3 …
  5. … fatique. The alloy offers excelent polishing caracteristics and ensures long tool life. … Replacement hips, knee parts, condyles, Gas …
  6. … no buffer layer except on materials considered critical or old hardsurfacing layers. In this Situation OA 4370, ER 100 SG  is recommended. …
  7. … deposition which offers high resistance to fatigue due to pressure and impact action in combination with abrasion. The martensitic … cutter pistons, shredder hammers, cutting tools, chain guides, running surfaces of heavily loaded PTO shafts, etc. … E DUR 600 Kb … 14700: E …
  8. … to oxidizing environments up to 1800°F (980°C) for prolonged exposures, and excellent resistance to sulfidation. It can be fabricated …
  9. … Very good deoxidization. Surfacing and joining of Copper and CuSn-Alloys. Widely used in oven … 6% tin for virtually all welding procedures. Very good deoxidisation. Surfacing and joining of Copper and CuSn-alloys. Widely used in oven …
  10. … losses. The slag is self lifting and leaves a fine rippled shiny surface. Max. service temperature 350ºC. Corrosion resistance similar …