Metal spray wires

Backoffice ID
9

SPA 750

SPA 750

Due to the high resistance to cracking and toughness, all spray metal requires no buffer layer except on materials considered critical. In this Situation Ceweld SP NiAl is recommended. Suited for wear parts subject to heavy abrasion. The interpass temperature should be maximum 250ºC. The spray deposit is machinable by special carbide tools.

SPA 760

SPA 760

Due to the high resistance to cracking and toughness, all spray metal requires no buffer layer except on materials considered critical. In this Situation Ceweld SP NiAl is recommended. Suited for wear parts subject to heavy abrasion. The interpass temperature should be maximum 250ºC. The spray deposit is machinable by special carbide tools. 

SPA 864

SPA 864

High wear resistance and simmilar structure as by C.-Cr. Carbide deposits. The deposit gives a very good hardness, all spray metal requires no buffer layer except on materials considered critical. In this Situation Ceweld SP NiAl is recommended. Suited for wear parts subject to extreme heavy abrasion. The spray deposit is only machinable by grinding. 

SPA 867

SPA 867

High wear resistance and simmilar structure as by C.-Cr. Carbide deposits. The deposit gives a extreme high hardness, all spray metal requires no buffer layer except on materials considered critical.  In  this  Situation Ceweld SP NiAl is recommended. The spray deposit is only machinable by grinding.

SPA 68T

SPA 68T

High wear resistance with ledeburitic structure as by C-Cr-B. Carbide deposits. The deposit gives a extreme high hardness, all spray metal requires no buffer layer except on materials considered critical. In this  Situation Ceweld SP NiAl is recommended. Suited for wear parts subject to extreme heavy abrasion and corrosion. Due to the high chromium content this alloy offers high heat resistance as well. The spray deposit is only machinable by grinding.