1. … alloyed steels, quenched and tempered for cementation and nitrating. Hydrogen content: HD < 5 ml/100 g weld metal … 13CrMoV42, 13CrMo4-4, …
  2. … make it weather resistant. Due to the seamless production process the hydrogen content is below 3ml/100g weld metal even after long storage …
  3. … Mpa) in case high impact values are required at sub zero temperatures. Hydrogen content HD < 4 ml/100 g. … Reh < 790 MPa  S620Q, S620QL, …
  4. … the alloy a preferred choice in many applications to prefent or solve problems. The wire is cleaned in a very special way to obtain porosity …
  5. … FL 830 ESH has an excellent slag removal. Flux has a low hydrogen potential which makes it suitable for overlay welding of heat …
  6. … conditioned by the high-basicity slag in combination with very low hydrogen content. Well suited for the economic joining of high strength … flux FL 155 should be used because of its high basicity and low hydrogen content. … Reh < 890 Mpa Iso 15608: 3.2 (Reh > 690 MPa) …
  7. … for high impact strength properties at extreme sub zero temperatures. Hydrogen content is less than HD < 4 ml/100gr weldmetal. … Reh ≤ 500 MPa ISO 15608: 1.2, 1.3, 2.1, 9.2  1.5637, …
  8. … 550 MPa yield strength, excellent welding properties and extreme low hydrogen content below HD 3 ml/100gr weld metal. The weldmetal is suitable for longer post weld heat treatments as applied …
  9. … constructions that needs post weld heat treatment after welding and still offers mechanical properties confirming 5Y46 class. Due to the seamless production process the hydrogen content is below 3ml/100gr weld metal even after long storage …
  10. … constructions that needs post weld heat treatment after welding and still offers mechanical properties confirming 5Y46 class. Due to the seamless production process the hydrogen content is below 3ml/100gr weld metal even after long storage …