1. … and petro- chemical processing, pulp and paper manufacturing, flue gas desulphurization systems and metal pickling operations. SA Alloy …
  2. … to seawater, thin acids and scale resistant in air and oxidizing gases up to 950°C . The weld deposit can be tempered and also can …
  3. … scale-resistant up to approx. 800°C in normal atmosphere and oxidizing gases. The weld deposit is capable of taking a high polish.Structure: …
  4. … scale-resistant up to approx. 800°C in normal atmosphere and oxidizing gases. The weld deposit is capable of taking a high polish … ISO 15608: …
  5. … life for several wear applications. Best to be used with shielding gas M13 (Argon with 1% Oxygen) approx. 15 litres per minute. … …
  6. … up to approx. 800 °C in normal atmosphere and oxidizing gases. The weld deposit is capable of taking a high polish … 1.4301, …
  7. … ducts, flame holders, thermocouple sheaths, and other important gas turbine components. … Haynes Alloy 230 … Alloy 230 Tig … A 5.14: …
  8. … which X-ray weld seams are reliably achieved both under CO2 and mixed gas … ISO 15608: 8.1  Austenit ≤ 19 % Cr , TÜV 1000: Gr. 21-30,  …
  9. … for semi and or semi–automatic applications. Weldable with Co2 and Mix gas. Suitable for creep resistant service for working temperatures up …
  10. … for semi and or semi–automatic applications. Weldable with Co2 and Mix gas.  … St 33 – St 52 ,A, E, AH, EH ,HI-HIII, 17Mn4, St 37.0/4 – St …