1. … Factor (X < 10 ppm) for temper embrittlement resistant applications. Fluxes FL 180 and FL 155 … Typ 1Cr0,5Mo, ISO 15608: ~5,1 1.7335, …
  2. … alternative for „stelliting“ . Best to be used with FL 8111 welding flux.  … Hot working tools such as: Stamping dies and Continuous …
  3. … to 1150 °C. When welding CEWELD 4820 AC low heat-input is required as alloys of such chemistry are sensitive to embrittlement at 600-800 °C. …
  4. … temperature creep resistance compared to standard CrMo creep resistant alloys. … For matching P92, 9%Cr1.7%W0.5%Mo, creep resisting …
  5. … CEWELD® AlSi12 Tig was originally developed as a brazing alloy to take advantage of its low melting point and narrow …
  6. … machined. CEWELD® SACW 4820 should be welded with CEWELD® FL 838 SAW flux. … 1.4340, 1.4710, 1.4745, 1.4746, 1.4712, 1.4762, 1.4713, 1.4773, …
  7. … Latest generation rutile flux cored wire, guarantees optimum metallurgical  quality, economic …
  8. … FL 160 is a highly basic SAW flux with low hydrogen content. Basicity: about 3 (according to …
  9. … Alloy: Sn94Ag6 / Solidus: 221°C / Liquidus: 279°C / Deposit color: Silver / Shear Strength (copper lap joint): 10,600 PSI … Copper, …
  10. … bead appearance without slag residues. Best to be used with welding flux FL 915 … 1.4317, 1.4313, 1.4407, 1.4414,    GX4CrNi13-4, …