1. …                           3 Layer: 61 - 65 HRc For the best results 2 till 3 layers should be welded. … Sugar mill knives and Hammers, Cement …
  2. … can be kept up to working temperatures of 600 ºC ; the hardness is still 40-45 HRc at these temperatures. For Hardfacing of more than 3 …
  3. … deposit is capable of taking a high polish. Structure: Austenite with delta ferrite. This fluxcored wire offers higher productivity, higher …
  4. … The weld deposit is offers strain hardening properties from 250 till 450 HB … austenitic manganese steel, high impact loads, hammers, …
  5. … 450°C and keep that also as interpass temperature. Slowly cooling down, for example in an oven. … 56-59 HRc hardfacing …
  6. … constructions that needs post weld heat treatment after welding and still offers mechanical properties confirming 5Y46 class. Due to the … 1.0475, 1.0416 to 1.0551 10Ni14, 12Ni14, 13MnNi6-3, 15NiMn6, S235JR-S355JR, S235JO-S355JO, S450JO, S235J2-S355J2, S275N-S460N, S275M-S460M, P235GH-P355GH, …
  7. … against heavy abrasion. Usualy the maximum number of layers is 2 till 3 but when using a special stringer build up technick with release …
  8. … constructions that needs post weld heat treatment after welding and still offers mechanical properties confirming 5Y46 class. Due to the …
  9. Deze hoge sterktestalen hebben hun hoge mechanische eigenschappen verkregen door de warmtebehandeling tijdens de vervaardiging. Het lassen van deze staalsoorten dient om deze reden zo dicht mogelijk aan te sluiten bij de oorspronkelijke warmtebehandeling (lees T8/5). In veel gevallen ondergaan deze …
  10. … constructions that needs post weld heat treatment after welding and still offers excellent impact properties. … P235GH, P265GH, P295GH, …