1. … where improved corrosion resistance in specific media is needed. In order to reduce the propensity for fissuring and hot cracking, the low …
  2. … gases. The weld deposit is capable of taking a high polish.Structure: Austenite with delta ferrite UNS 34780 … ISO 15608: 8.1 / TüV Groupe 29 …
  3. … Preheating and interpass temperature 400-450 °C (austenitic welding) or 250-300 °C (martensitic welding). Root passes …
  4. … abrasion. This alloy has no risk for cracks and can also be applied on austenitic manganese steels. The weld deposit is good machinable. Very …
  5. … but was then adapted for application as a material for the steam headers to which the boiler tubes are connected. … Inconel alloy 740H … …
  6. … gases. The weld deposit is capable of taking a high polish. Structure: Austenite with delta ferrite. This fluxcored wire offers higher …
  7. … CEWELD® L-Ag49niMn is a very good flowing, low-melting silver hard solder for operating temperatures from -200 °C to Max. 200 °C (without …
  8. … Fully austenitic weld metal with high resistance against stress corrosion …
  9. … where improved corrosion resistance in specific media is needed. In order to reduce the propensity for fissuring and hot cracking, the low …
  10. … responsible for its creep strength are kept above the minimum considered necessary to ensure satisfactory performance. In this case, …