1. … Outstanding alloy against high impact combined with abrasion including metal to metal friction. The weld … appearance and outstanding welding properties on both AC and DC+. Preheating is not required. … Rebuilding worn machine parts, Rails, …
  2. … Mechanical properties listed below reflect utilization of a post-weld … between 1024°C (1875°F) and 1052°C (1925°F) for one hour, followed by precipitation hardening between 623°C (1135°F) … Suitable for precipitation hardening stainless steel used for welding materials of …
  3. … The presence of tin improves the fluidity and is useful to increase the activity of the flux. Do not use this alloy above working temperatures …
  4. … High pressure resistance and high wear resistance. The alloy is characterized by very low thermal electromotive force (emf) compared to …
  5. … NiCrMo 686 (UNS N06686/W.Nr. 2.4606) is a single-phase, austenitic … to enhance properties. Low carbon (C) helps minimize grain boundary precipitation to maintain corrosion-resistance in the heat-affected … and super-austenitic stainless steels, nickel alloys such as UNS N06059 and N06022, INCONEL alloy C-276, and INCONEL alloys 622, C22, 625, …
  6. CEWELD AquaForce MG offers a high deposition rate with remarkable … exceeding 500 MPa in sweet and salt water makes AquaForce MG the preferred choice by professional divers. … Reh ≤420 MPa (60 ksi) ISO 15608: 1.1, 1.2 1.0035, 1.0570, 1.0461,1.0562, …
  7. … Very good abrasion resistance in combination with impact even at higher temperatures up to 550ºC. To much layers should be avoided, preheat is necessary to avoid cracking. A buffer layer with AA M690 or …
  8. … Outstanding alloy against high impact combined with abrasion including metal to metal friction. The weld … appearance and outstanding welding properties on both AC and DC+. Preheating is not required. … Rebuilding worn machine parts, Stone …
  9. … Excellent weldabillity and good mechanical strength combined with good … alloys and covers a weight range of alloys. Thicker sections should be preheated (150°C) prior to welding. Qualified by Lloyds for manual and … 3.3211, 3.4335, EN AW 5086, EN AW 5083, EN AW 5019, EN AW 5019, EN AW 6060, EN AW 6005A, EN AW 6082, EN AW 6061, EN AW 7020, EN AC 51300, EN …
  10. … De nombreuses années d'essais de nouvelles compositions de rechargement ont permis d'obtenir un nouveau fil de soudure spécial pour Nihard, d'une durée de vie exceptionnelle Après 1547 heures …