1. … High pressure resistance and high wear resistance. The alloy is characterized by very low thermal electromotive force (emf) compared to …
  2. … NiCrMo 686 (UNS N06686/W.Nr. 2.4606) is a single-phase, austenitic … to enhance properties. Low carbon (C) helps minimize grain boundary precipitation to maintain corrosion-resistance in the heat-affected … and super-austenitic stainless steels, nickel alloys such as UNS N06059 and N06022, INCONEL alloy C-276, and INCONEL alloys 622, C22, 625, …
  3. … Outstanding alloy against high impact combined with abrasion including metal to metal friction. The weld … appearance and outstanding welding properties on both AC and DC+. Preheating is not required. … Rebuilding worn machine parts, Rails, …
  4. … Very good abrasion resistance in combination with impact even at higher temperatures up to 550ºC. To much layers should be avoided, preheat is necessary to avoid cracking. A buffer layer with AA M690 or …
  5. CEWELD AquaForce MG offers a high deposition rate with remarkable … exceeding 500 MPa in sweet and salt water makes AquaForce MG the preferred choice by professional divers. … Reh ≤420 MPa (60 ksi) ISO 15608: 1.1, 1.2 1.0035, 1.0570, 1.0461,1.0562, …
  6. … Excellent weldabillity and good mechanical strength combined with good … alloys and covers a weight range of alloys. Thicker sections should be preheated (150°C) prior to welding. Qualified by Lloyds for manual and … 3.3211, 3.4335, EN AW 5086, EN AW 5083, EN AW 5019, EN AW 5019, EN AW 6060, EN AW 6005A, EN AW 6082, EN AW 6061, EN AW 7020, EN AC 51300, EN …
  7. … De nombreuses années d'essais de nouvelles compositions de rechargement ont permis d'obtenir un nouveau fil de soudure spécial pour Nihard, d'une durée de vie exceptionnelle Après 1547 heures …
  8. … Submerged arc welding wire for welding fine grain steels for low temperature requirements down to -60°C in apparatus, construction and offshore applications. …   … 19Mn5 St 35.8, St 45.8 StE 210.7 TM, StE 480.7 TM StE 255 to StE 460 X 42, X65, X 70 EN same S185 - S355-S460 P235GH, P355GH P235T1/T2, …
  9. … Outstanding alloy against high impact combined with abrasion including metal to metal friction. The weld … appearance and outstanding welding properties on both AC and DC+. Preheating is not required. … Rebuilding worn machine parts, Stone …
  10. CEWELD 430 Ti is a 18%Cr alloy stabilized with Ti. This alloy has improved oxidation and corrosion resistance over an ER409 alloy. Single pass welds on light gage base metal or welds with preheat do not usually require PWHT. … 1.4000, 1.4002, 1.4016, 1.4057, …