1. … properties and no limmits in the number of layers. The deposit is non magnetic and can not be flame cut.  … Rebuilding, buffer layers, …
  2. … Austenitic, non magnetic stainless steel alloy with high mechanical properties and …
  3. … Sound, pore free deposits on ferrous and non-ferrous base materials offering excellent resistance to corrosion …
  4. … properties and no limits in the number of layers. The deposit is non magnetic and can not be flame cut. … Rebuilding, buffer layers …
  5. … stainless steel, DUR 6 can be used to protect bearing surfaces in non-lubricating conditions due to its resistance to metal-to-metal …
  6. … means that this steel is distinctly vulnerable to sensitization phenomenon during welding, even though martensite hogs a great amount of …
  7. … bright, almost smut-free welds. Not recommended for anodizing. Non-heat treatable. Thicker sections should be preheated (150°C) prior …
  8. … 50 kVA et notre machine à induction ProHeat 35 avec Rolling Inductor, pour le préchauffage du manipulateur. Outre l'exécution de ces …
  9. … high Mo. content. Suitable for use up to 400 °C. The weld deposit is non magnetic. … Designed for joining corrosion resistant CrNiMoN steel …
  10. … sont listés dans cette brochure, veuillez remplir le formulaire pour recevoir le PDF. … Téléchargement de catalogue …