1. … that are organized periodically. Themes such as stainless steel, nickel, aluminum, copper, cladding and welding economics have already …
  2. … puddle. This wire offers a unique welding deposit with more than 1% nickel and 0,5% Cu due to the seamless production process the hydrogen …
  3. … in the first layer. A buffer layer is recommended in case of sensible base material or old layers. Weldable without protective gas … 63-67 …
  4. … combined with high strength due to the addition of copper. The filler metal shows remarkable bonding properties and fluididity during …
  5. Brand: Selectarc
    CEWELD Product: SG Ni2,5
    … Existe en TIG … 52 … SELECTARC F82 …
  6. … Usually combined with AlSi12 or AlSi5 filler metal. … Brazing for Aluminium and Aluminium Alloys with a … range from 350 to 550 °C. Usually combined with AlSi12 or AlSi5 filler metal. … Alu-Flux … 18496: FL20 …
  7. … Cu-Al-Ni bronze. Sound, pore free deposits on ferrous and non-ferrous base materials. Seawater, wear and corrosion resistance; for example … pressure. Especially suited for marine environments. The addition of nickel improves corrosion resistance in heat and rough seawater. … …
  8. … All CEWELD® products are listed in this brochure, please fill in the form to receive the PDF. … Catalog download …
  9. … superalloys. CEWELD® Alloy 263 is an age-hardenable nickel-cobalt-chromium-molybdenum alloy designed specifically to … age cracking problems common for gamma prime strengthened alloys.  … NIckel based alloys with simmilar composition as Nimonic 263 … Alloy 263 …
  10. … currents. Using temperature down to - 40 °C. Particularly suited for MAG-orbital welding and all-position welding on ceramic backing. …