1. … of sulfuric acid and many chloride containing media. This filler metal may also find applications for joining Type 317L material where …
  2. … Absolutely crack resistant weld metal conditioned by the high-basic slag in combination with very low …
  3. … age hardenable deposit and similar mechanical properties as the base metal. Age hardened condition: 720ºC for 8 Hours, furnace Cool 55ºC/ …
  4. … in the molten weldpool and become part of the weld deposit, Metal core fluxcored wires are recommended in spray arc to obtain the …
  5. … steam pipes and similar joints made of Cr-Mo alloyed steel. The weld metal is resistant to working temperatures up to 550°C. as for …
  6. … non-oxidizing liquids and are recommend for internal and external diameters. Using the combustion wire spray process, CEWELD® SP 1.4302 …
  7. … Crack resistant weld metal conditioned by the high-basicity slag in combination with very …
  8. … Remarkable crack resistant weld metal in combination with very low ( …
  9. … has better elevated temperature properties than Grade 2 or 3 and is sometimes specified for pressure vessels or piping for its superior …
  10. … Due to the high resistance to cracking and toughness, all spray metal requires no buffer layer except on materials considered critical. …