- … The weld seam shows a fine rippled surface free from inclusions and undercut. … Buffer and build up layers prior to hardfacing and or build …
- … alter the surface electrochemistry of the material in the crevice or under a surface deposit. Grade 12 has better elevated temperature …
- … all weld metal requires no buffer layer except on materials considered critical. Suited for wear parts subject to heavy impact and … first layer. … Conveyors and transport surfaces, tires, bucket and loader teeth, cruscher jaws, Bufferlayers, crane wheels, axis, gear parts, …
- … at very low currents. It is easy to use and inexperienced welders will have no difficulties to produce smooth deposits mainly …
- … quality guarantees optimum metallurgical quality and attractive welder appeal. The weld deposit meets the NiCrFe-3 requirements. Better …
- … There are many ways to make prior tests for welding joints in order to find the weakest spots and also lots of standards that have to …
- … quality guarantees optimum metallurgical quality and attractive welder appeal. Combined with our high basic electro slag flux FL 830 ESHC …
- … better mechanical characteristics compare to standard PbSn soft solders. Excellent results are obtained on stainless steel with our "ST" …
- … and joining of Copper and CuSn-Alloys. Widely used in oven soldering. High quality alloyed copper wire. Sound, pore free deposits and … and joining of Copper and CuSn-alloys. Widely used in oven soldering. Mat.n: 2.1010, 2.1016, 2.1020, 2.1030, 2.1050, 2.1052, 2.1056, …
- … where improved corrosion resistance in specific media is needed. In order to reduce the propensity for fissuring and hot cracking, the low …