1. … High chromium-alloyed welding wire (ER 327-ER 329) based on a 25% Chromium and 4% Nickel deposit for cladding and joining …
  2. … Silicon bronze • Sound, pore free deposits on ferrous and non-ferrous base materials • Excellent corrosion resistance  … Welding thin steel …
  3. … tools, hardening is possible. The maximum hardness is dependent on the base metal and is often achieved in the first layer. … Rebuilding worn …
  4. … dilution of the electro slag process. Due to the low dilution with the base metal a hardness exceeding 50 HRc can be achieved already in the …
  5. … 815 °C (1500°F) up to 1149 °C (2100°F), especially when welding on base metals of nickel-iron-chromium alloys. … Inconel alloys 600 and …
  6. … post-weld heat-treatment are required . AA 410 is a martensitic stainless steel that is heat-treatable. It has a nominal weld metal …
  7. … Vanadium to give improved long term creep properties. These consumables are specifically intended for high integrity structural service at …
  8. … Special alloy for welding aluminium-magnesium based alloys with maximum 5% Mg. Zirconium added as grain refiner to …
  9. … Cu-Al-Ni bronze. Sound, pore free deposits on ferrous and non-ferrous base materials. Seawater, wear and corrosion resistance; for example …
  10. … in the first layer. A buffer layer is recommended in case of sensible base material or old layers. Weldable without protective …