1. … plate less than 1/4 in. thick to prevent oxidation. Gas Requirements. Welding-grade argon (99.999 percent purity) usually is chosen for … gas supply should not be more than -60 degrees F (-51 degrees C). … Welding Zirconium alloys in general but also for successfully weld zirconium to titanium, …
  2. … Excellent welding characteristics and easy slag removal with remarkable out of …
  3. … resistance against seawater and general corrosion with excellent welding properties with self detaching slag.  … NF A 35-578 : Z 15 CN …
  4. … A stainless steel alloy for the assembly and cladding of 17% chromium alloys and age Hardfacing components where heat and corrosion …
  5. … Stainless steel alloy for joining and cladding 17% Chromium alloys and cladding components where heat and corrosion resistance …
  6. … corrosion-resistance in a range of severe environments. Its high nickel (Ni) and molybdenum (Mo) provide good resistance in reducing … … Duplex, super-duplex and super-austenitic stainless steels, nickel alloys such as UNS N06059 and N06022, INCONEL alloy C-276, and …
  7. … Excellent welding properties with high build-up capacity and low dilution rate. …
  8. … structural steels with yield strength of Rp0,2 550 MPa (80 ksi). As welding flux we recommend our type FL 155, classification S A FB 1 55 …
  9. … and weldability, better wetting properties compared to solid wires.Excellent weld metal quality and X-ray soundness and excellent …
  10. … against abrasion is 4 till 8 times better in comparison with C-Cr alloys … Sinter plant parts, Swing hammers, Drilling surfaces, Stone …