1. … Fully austenitic weld metal with high resistance against stress corrosion …
  2. … gases. The weld deposit is capable of taking a high polish.Structure: Austenite with delta ferrite … ISO 15608: 8.1 / TüV Groupe 29 (+22+21) …
  3. … A high basic electrode for welding austenitic-ferritic stainless alloys of the 22% Cr, 5% Ni, 3% Mo …
  4. … rutile slag with which X-ray weld seams are reliably achieved both under CO2 and mixed gas … ISO 15608: 8.1  Austenit ≤ 19 % Cr , TÜV 1000: Gr. 21-30,  1.4583, 1.4435, 1.4436, …
  5. … where improved corrosion resistance in specific media is needed. In order to reduce the propensity for fissuring and hot cracking, the low …
  6. … L-Ag27 is a Very good flowing, low-melting silver hard solder for operating temperatures from -200 °C to Max. 200 °C (without …
  7. … responsible for its creep strenghth are kept above the minimum considered necessary to ensure satifactory performance. … For matching P91, …
  8. … über unsere Tagungseinrichtungen und B2B-Veranstaltungen oder Beratung wenden Sie sich bitte an: Patrick Bovendeerd Tel: +31 (06) …
  9. … to apply alloy without any risk for cracks and can also be applied on austenitic manganese steels. The weld deposit is machinable with …
  10. Austenitic deposit with strain hardening properties and no limits in …