- … Mo content, with low carbon content (less than 0.05%), to be used for welding creep resistant steels. … For 2.5%Cr-1%Mo-alloyed, …
- … Excellent welding characteristics and easy slag removal with remarkable out of …
- … Submerged arc welding wire for high temperature creep resistant 2,45%Cr 1,0%Mo …
- … offer low hydrogen content and excellent weldabillity in multi layer welding and narrow gab. … X80, AISI 4130, 8630, ASME: ASTM A302 Grade …
- … cored wire have a excellent weld puddle. This wire offers a unique welding deposit with more than 1% nickel and 0,5% Cu due to the …
- … self lifting slag and improved coating against moisture pick up. Welding instructions: Start the electrode with about 130% hot start and …
- … and oxidation resistance above 1150 °C ( 2100 °F), especially when welding on base metals of nickel-iron-chromium alloys. High mechanical …
- … A continuous, solid, corrosion-resistant, duplex wire for welding austenitic-ferritic stainless alloys of the 22% Cr, 5% Ni, 3% …
- … FL 805 is an agglomerated flux for SAW welding stainless steels and Nickel based alloys: AISI 2205, Alloy 625, … Grain size: 2-16 … chromium compensated flux for submerged arc welding of stainless steel grades … FL 805 … 14174: SA AF 2 5644 DC H5 …
- … treatable. Thicker sections should be preheated (150°C) prior to welding. … G-AlSi10Mg, G-AlSi11, G-AlSi12 (Cu), G-AlSi7Mg, G-AlSi6Cu4, …