1. … A copper coated, Ni-alloyed (2,4% Ni), solid wire for low temperature … of 470 MPa. The wire provides excellent impact toughness down to -60°C. … For cryogenic construction steels and Ni bearing low temperature steels.   11MnNi5-3, 13MnNi6-3, 15NiMn6, S275NL-S460NL, S275ML-S460ML, P275NL2-P460NL2, P355ML2-P460ML2 ASTM: A203 grade …
  2. … Das Team von Welding Solution Center kreiert und organisiert Ihr Business Event. Während des gesamten Prozesses haben Sie einen Ansprechpartner, der mit Ihnen eine Reihe von Phasen bespricht, damit Sie Ihr …
  3. … He is a copper coated, Ni-alloyed (2,4% Ni), solid wire for low temperature … of 470 Mpa. The wire provides excelent impact thoughness down to -60°C. … For cryogenic construction steels and Ni bearing low temperature steels. 11MnNi5-3, 13MnNi6-3, 15NiMn6, S275NL-S460NL, S275ML-S460ML, P275NL2-P460NL2, P355ML2-P460ML2 ASTM: A203 grade …
  4. CEWELD E NiFe 2 has a few benefits compare to other “FeNi” types … free from porosity even on old and or otherwise diluted base material. Preheating is normally done to slow down the cooling speed, in case you … EN-GJS-400-15, EN-GJS-400-18, EN-GJS-450-10, EN-GJS-500-7, EN-GJS-600-3, EN-GJS-700-2. GGG40, GGG45, GGG50, GGG60; GGG70, GGG80   … E …
  5. … NiCrMo 686 (UNS N06686/W.Nr. 2.4606) is a single-phase, austenitic … to enhance properties. Low carbon (C) helps minimize grain boundary precipitation to maintain corrosion-resistance in the heat-affected … and super-austenitic stainless steels, nickel alloys such as UNS N06059 and N06022, INCONEL alloy C-276, and INCONEL alloys 622, C22, 625, …
  6. … Outstanding alloy against high impact combined with abrasion including metal to metal friction. The weld … appearance and outstanding welding properties on both AC and DC+. Preheating is not required. … Rebuilding worn machine parts, Rails, …
  7. … Mechanical properties listed below reflect utilization of a post-weld … between 1024°C (1875°F) and 1052°C (1925°F) for one hour, followed by precipitation hardening between 623°C (1135°F) … Suitable for precipitation hardening stainless steel used for welding materials of …
  8. CEWELD® 316H is designed for welding 316/316H austenitic stainless … in thick highly restrained weldments, since the possibility of premature service failure by intergranular HAZ cracking is reduced by using more ductile weld metal rather than 347H. … ISO 15608: 8.1  Austenit ≤ 19 % Cr , TÜV 1000: Gr. 21, 22, 24,  1.4401, …
  9. CEWELD AquaForce MG offers a high deposition rate with remarkable … exceeding 500 MPa in sweet and salt water makes AquaForce MG the preferred choice by professional divers. … Reh ≤420 MPa (60 ksi) ISO 15608: 1.1, 1.2 1.0035, 1.0570, 1.0461,1.0562, …
  10. … Very good abrasion resistance in combination with impact even at higher temperatures up to 550ºC. To much layers should be avoided, preheat is necessary to avoid cracking. A buffer layer with AA M690 or …