1. … carbon, silicon, and phosphorus are controlled to lower levels in this alloy. … 1.4465, 1.4500, 1.4505, 1.4506, 1.4519, 1.4531, 1.4536, …
  2. … carbon, silicon, and phosphorus are controlled to lower levels in this alloy. Suitable in all positions. … 1.4465, 1.4500, 1.4505, 1.4506, …
  3. … 2400 HV Iron and Tungsten based hardfacing alloy containing 52-58% (depending on wire diameter) tungsten carbides. …
  4. Alloy: Sn94Ag6 / Solidus: 221°C / Liquidus: 279°C / Deposit color: …
  5. … grade of the Al-Bronze-types. Seawater-resistant copper-aluminum alloy without Zn with high toughness and improved hardness.  “Very good …
  6. … Aluminium alloyed tubular wire for electric arc spray on a Fe-Al basis with high …
  7. … losses of brazed joints with lower silver containing Phosphor-Copper Alloys. Ideal where the heat feeding is critical because of its low … … Copper to Copper (without flux). Brass, Copper and Copper-Tin Alloys (with flux). Do not use in a sulphurous environment. … L-Ag18PL …
  8. … Outstanding alloy against abrasion, impact and high temperatures up-to 550 °C. The …
  9. … Due to the addition of 0,5% copper and 0,8% Ni this alloy offers excellent weather resistant properties … CuNi, Reh ≤ …
  10. … • High quality alloyed copper wire for the Tig process (Mig brazing as well) • The … plates in the car industry and also for cladding CuMn, CuSiMn and CuZn alloys. Suitable for cladding cast iron and un- and low alloyed steels. Sislicon Alloy: 2.0220 - CuZn 5, 2.0230 - CuZn 10, …