1. … and excellent ductility.  Long term use at working temperatures between 600°C and 800°C should be avoided. … Ni 6625 / NiCr22Mo9Nb / 2.4831 …
  2. … CEWELD 308H has been developed for typical operating temperatures up to 400ºC, and up to …
  3. … listed below reflect utilization of a post-weld heat treatment between 1020°C (1875°F) and 1050°C (1925°F) for one hour, followed by precipitation hardening between 612°C (1135°F) … Suitable for precipitation hardening stainless …
  4. … listed below reflect utilization of a post-weld heat treatment between 1024°C (1875°F) and 1052°C (1925°F) for one hour, followed by precipitation hardening between 623°C (1135°F) … Suitable for precipitation hardening stainless …