1. … to crack, especially if the weld seams are not heat-treated.These steels are usually used for operating temperatures of up to 550°C. … … For similar 1.25%Cr-0.5%Mo-alloyed, heat-resistant, ferritic steels. 1.7335, 1.7242, 1.7337, 1.7357 13CrMo 4-5, 13CrMo 4-4, 16 …
  2. … for welding fine grained similar alloyed high yield strength steel > 960 MPa in case high impact values are required at sub …
  3. … Root is a thick basic-rutile coated electrode for welding low alloyed steels with tensile strength up to 510 N/mm2. Recommended for root …
  4. … is a bronzed wire to offer excellent feeding properties with standard steel liners. … S185-E360, S235JR-S355JR, S235J0-S450J0, S235J2-S355J2, …
  5. … A stainless steel alloy for the assembly and cladding of 17% chromium alloys and … offers high hardness and wear resistance. … 1.4122 (G)X35CrMo17, Cast steels … MA 4115 … A 5.9: ER430 … 14343-A: G 17 …
  6. … Ceweld SP NiAl is recommended. Suited for wear parts subject to heavy abrasion. The interpass temperature should be maximum 250ºC. The …
  7. … Corrosion resistance is higher than 5%Cr-0.5%Mo steels requirements. To be used with shielding gas Ar+O2.   … For matching 9%Cr-1%Mo creep resisting martensitic steels ASTM: A182 Gr F9, A199 Gr T9 , A213 Gr T9 , A217 Gr C12 , A234 …
  8. … It has cavitation-erosion resistance ten times that of 304 stainless steel, Dur 12 can be used to protect bearing surfaces in …
  9. … in case of rebuilding but heat input should be kept low (as for Mn steel, interpass temperature should be kept < 250 °C). … Rebuilding and joining cold straining Mn steels or rebuilding parts that are subject to high impact and rolling …
  10. … offers excellent weldability when properly cleaned prior to welding. Heavy parts and thicker plates should be preheated (150°C), prior to …